초록
The stone lantern of the Damyang Gaeseonsaji temple site is a cultural heritage built during the Unified Silla period (AD 868). The reason for its value as a cultural property is due to wittern the background and the period created on inscription of the lamp stone engraved by letters. The stone lantern consists of two types of lithic tuffs for the 23 original properties, the replaced stones in 1991, and the biotite granite for its ground stones replaced in 2005. The lithic tuffs selected as the replacement parts in 1991 and 2017 have been examined and got to properties of hardly exposure moisture as well as very similar geochemical characteristics. There were various types of physical deterioration of the stone properties and structural cracks; in particular, on the northern side of the stylobates. Chemical and biological deterioration can be identified as black, white, and brown discolorations as well as by the presence of lichens, bryophytes, and herbaceous plants. In the evaluation of the physical properties of the stone lantern, the mean and maximum ultrasonic velocities were found to be similar in each direction. However, the lowest velocity on the east and south sides were found to be lower than those of other stone properties. It was found that physical damage to the stylobates resulted from water expansion in a freeze-to-thaw phenomena related to water content. Therefore, dismantling repair was carried out in the protection facility to restrict further water supply to the stone as much as possible.
Abstract
The stone lantern of the Damyang Gaeseonsaji temple site is a cultural heritage built during the Unified Silla period (AD 868). The reason for its value as a cultural property is due to wittern the background and the period created on inscription of the lamp stone engraved by letters. The stone lantern consists of two types of lithic tuffs for the 23 original properties, the replaced stones in 1991, and the biotite granite for its ground stones replaced in 2005. The lithic tuffs selected as the replacement parts in 1991 and 2017 have been examined and got to properties of hardly exposure moisture as well as very similar geochemical characteristics. There were various types of physical deterioration of the stone properties and structural cracks; in particular, on the northern side of the stylobates. Chemical and biological deterioration can be identified as black, white, and brown discolorations as well as by the presence of lichens, bryophytes, and herbaceous plants. In the evaluation of the physical properties of the stone lantern, the mean and maximum ultrasonic velocities were found to be similar in each direction. However, the lowest velocity on the east and south sides were found to be lower than those of other stone properties. It was found that physical damage to the stylobates resulted from water expansion in a freeze-to-thaw phenomena related to water content. Therefore, dismantling repair was carried out in the protection facility to restrict further water supply to the stone as much as possible.
참고문헌 (24)
- Research of repairs for cultural heritage of Korea in 1991, "Cultural Heritage Administration", 763~793 (1993)
- Fitzner, B., "Damage diagnosis on stone monuments—Weathering forms, damage categories and damage indices", Stone Weathering and Atmospheric Pollution Network (SWAPNET), 11~56 (2001)
- Fitzner, B., "Weathering damage on Pharaonic sandstone monuments in Luxor-Egypt", Building and Environment, 38(9-10), pp.1089~1103 (2003)
- Govindaraju, K., "Compilation of working values and samples description for 272 geostandards", Geostandards Newsletter, 13(Special), pp.1~113 (1989)
- Iliev, I. G., "An attempt to estimate the degree of weathering of instructive rocks from their physicomechanical properties", International Society for Rock Mechanics and Rock Engineering, 109~114 (1966)
- 조영훈, "석조문화유산의 손상지도 제작방법과 표면 및 3차원 손상율 평가기법", 보존과학회지, 27(3), pp.251~260 (2011), 한국문화재보존과학회
- 조영훈, "석조문화유산의 박리검출을 위한 수동적 적외선 열화상분석의 적용성 연구", 보존과학회지, 29(1), pp.55~67 (2013), 한국문화재보존과학회[DOI]
- Jo, Y. H., "Quantitative modeling of blistering zones by active thermography for deterioration evaluation of stone monuments", Journal of Cultural Heritage, 15(6), pp.621~627 (2014)
- 조영훈, "석조문화유산의 표면 요철도에 적합한 초음파 탐촉자 및 접촉매질 선정 연구", 보존과학회지, 31(3), pp.267~278 (2015), 한국문화재보존과학회
- Kahraman, S., "Estimating the direct P-wave velocity value of intact rock from indirect laboratory measurements", International Journal of Rock Mechanics and Mining Sciences, 39(1), pp.101~104 (2002)
- Kim, Y. H., "The Compilations of archaeological data in Korea. Atlas of archaeological sites in Joseon dynasty 4", National Culture, 4, pp.500~501 (2005)[DOI]
- Koo, M. H., "Review of the engraving record in stone lantern of Gaeseonsaji temple site at Damyang—Focused on land deal case of the 9th century in United Silla Kingdom", The Journal of History and Practical Thought Studies, 15⋅16, pp.59~80 (2000)[DOI]
- Lee, C. H., "Correlation and correction factor between direct and indirect methods for the ultrasonic measurement of stone samples", Environmental Earth Science, 76(14), pp.477~489 (2017)
- 이찬희, "부여 정림사지 오층석탑 구성암석의 원산지 추정", 지질학회지, 43(2), pp.183~196 (2007), 대한지질학회
- 이찬희, "석조문화재 풍화도 평가를 위한 초음파 측정의 설정과 직접-간접전달방법의 상관관계", 보존과학회지, 25(3), pp.233~244 (2009), 한국문화재보존과학회
- 이찬희, "중원탑평리칠층석탑의 재질특성과 산지추정 및 손상도 진단을 통한 보존처리", 헤리티지:역사와 과학, 43(3), pp.4~25 (2010), 국립문화유산연구원
- 이찬희, "울산 반구대암각화의 손상도 및 사면안정성 평가", 보존과학회지, 28(2), pp.153~164 (2012), 한국문화재보존과학회[DOI]
- Identification of frost susceptible particles in concrete aggregates, "National Highway Cooperative Research Program", 1~62, pp.Report 66 (1969)
- Research of stone lanterns in Korea. Ⅱ, "National Research Institute of Cultural Heritage", 13~29 (2001)
- Nockolds, S. R., "Average chemical compositions of some igneous rocks", Bulletin of the Geological Society of America, 65(10), pp.1007~1032 (1954)
- 박성미, "화순 운주사 원형다층석탑의 재질특성과 훼손도 평가", 헤리티지:역사와 과학, 45(1), pp.86~101 (2012), 국립문화유산연구원[DOI]
- Pearce, J. A., "Continental basalts and mantle xenolith", pp.230~349 (1983), Shiva
- Taylor, S. R., "The continental crust: Its composition and evolution", pp.312~312 (1985), Blackwell
- Uchida, E., "Consideration on the construction process and the sandstone quarries during the Angkor period based on the magnetic susceptibility", Journal of Archaeological Science, 34(6), pp.924~935 (2007)